5083 Precision-Slit Aluminum Strip: Widths to ±0.05 mm, Tempers, Coil Sourcing & Pricing
HXM slits 5083 aluminum strip from our own master coils: 0.15–6.0 mm thick, 3–1,300 mm wide, width tolerance to ±0.05 mm, in O / H12 / H14 / H16 / H18 / H32 / H34 tempers with burr-free slit edges. Strip is the form buyers choose when they need marine-grade corrosion resistance in narrow, tight-tolerance lengths — cable armouring, transformer and choke cases, marine panel stiffeners, gaskets and stamped brackets. MOQ 500 kg, EN 10204 3.1 certificate with every coil, quotation within 24 hours.
⚡ Quick Answer
5083 strip is simply 5083 coil slit to narrow width — the same 4.0–4.9 % Mg chemistry that makes 5083 the marine-grade benchmark, delivered in widths your stamping, winding or armouring line can feed directly. Pick O for deep forming and armouring, H32/H34 for stamped brackets and panels, H18 where maximum strip strength is needed. Because 5083 work-hardens faster than 5052, order it when your part needs 30 % more strength than 5052 strip in the same temper. See the full strip range for sibling alloys.
5083 Strip Specifications at a Glance
Everything a sourcing engineer needs to judge feasibility before sending an RFQ:
| Parameter | Range / Value | Note |
|---|---|---|
| Alloy | 5083 (EN AW-5083 / AlMg4.5Mn0.7 / UNS A95083) | ASTM B209 · EN 485 · GB/T 3880 |
| Thickness | 0.15 – 6.0 mm | gauge conversions in our gauge guide |
| Width | 3 – 1,300 mm slit; master coil up to 2,500 mm | custom widths standard |
| Width tolerance | ±0.05 mm standard; ±0.02 mm on request | laser-measured per coil |
| Thickness tolerance | ±1–5 % of thickness by class | special class available |
| Tempers | O, H12, H14, H16, H18, H32, H34 | EN 515 designations |
| Edge | slit (standard), deburred edge on request | burr ≤ 0.05 mm |
| Core & packing | steel/aluminium core 200/300/400/500 mm | moisture-barrier wrap |
| Coil weight | 100–3,000 kg per slit coil | OD up to 1,600 mm |
| Certification | EN 10204 3.1 mill certificate | marine class certs on request |
| MOQ | 500 kg per width-thickness combination | trial widths from stock masters |
| Lead time | 12–25 days | faster from running stock widths |
Why Specify 5083 as Strip — and When 5052 or 3003 Beats It
Strip buyers juggle three competing alloys. Here is the honest decision matrix our sales engineers use:
| Factor | 5083 strip | 5052 strip | 3003 strip |
|---|---|---|---|
| Strength (O temper) | 275–350 MPa | 170–215 MPa | 110–130 MPa |
| Formability | Good (O/H12) | Excellent (O) | Excellent |
| Seawater corrosion | Outstanding | Excellent | Moderate — not for immersion |
| Cost per tonne | highest | mid | lowest |
| Work-hardening rate | high — strength rises fast with temper | moderate | low |
| Best for | marine hardware, cable armour in splash zones, high-load stamped parts | general formed parts, tanks, trim | transformer windings, HVAC, deep drawing |
Rule of thumb: if the part sees seawater and load, 5083 strip pays for itself. If it only needs corrosion protection without structural load, 5052 strip is usually the smarter spend. For indoor electrical or HVAC work, 3003 strip wins on cost. Full alloy comparisons: 5052 vs 5083 buyer’s guide.
Chemical Composition (EN 573-3 / ASTM B209)
| Element | Min (%) | Max (%) |
|---|---|---|
| Mg | 4.0 | 4.9 |
| Mn | 0.40 | 1.00 |
| Cr | 0.05 | 0.25 |
| Si | — | 0.40 |
| Fe | — | 0.40 |
| Cu | — | 0.10 |
| Zn | — | 0.25 |
| Ti | — | 0.15 |
| Other each / total | — | 0.05 / 0.15 |
| Aluminium | remainder | — |
The high Mg + Mn combination is what gives 5083 strip its strength-per-micron advantage — critical when your design is thickness-limited but load-bearing.
Mechanical Properties by Temper (EN 485-2)
| Temper | Tensile strength (MPa) | 0.2% proof (MPa) | Elongation A50 |
|---|---|---|---|
| O | 275–350 | ≥125 | ≥16 % |
| H12 | ≥305 | ≥145 | ≥9 % |
| H14 | ≥340 | ≥230 | ≥6 % |
| H16 | ≥370 | ≥280 | ≥4 % |
| H18 | ≥410 | ≥330 | ≥3 % |
| H32 | ≥305 | ≥215 | ≥7 % |
| H34 | ≥340 | ≥250 | ≥5 % |
Values for common strip gauges; actuals per heat appear on the mill certificate. Cross-alloy strength data: aluminum mechanical properties chart · temper logic: temper designations explained.
Temper Selection by Application — and What Seawater Does to Strip
| Application | Recommended temper | Reason |
|---|---|---|
| Cable armouring / interlocking | O | Maximum ductility — armour profiles form without edge cracking |
| Deep-formed cases & housings | O / H12 | Formability first; strength recovers in final part geometry |
| Marine stiffeners & trims | H32 / H34 | Structural stiffness on wide spans |
| High-strength stamped clips | H34 | 250 MPa proof strength holds fastener loads |
| Springs & retaining rings | H18 | 410 MPa class from work hardening alone |
| Welded strip assemblies | H32 | Predictable HAZ behaviour with ER5356/5183 filler |
Corrosion behaviour mirrors the plate data: 5083’s high-magnesium chemistry gives outstanding splash-zone and immersion performance, with copper held ≤0.10 % so no galvanic cells form inside your assembly. For armouring and marine trims we add lot-by-lot exfoliation-corrosion screening on request — same ASTM G34 protocol used on hull plate. Background: does aluminum rust? corrosion guide.
Slitting Capability — Width Tolerance, Edge Quality & Camber
Strip is a tolerance business. This is exactly what HXM’s slitting lines hold, coil after coil:
| Attribute | Standard | Premium (on request) |
|---|---|---|
| Width tolerance | ±0.05 mm | ±0.02 mm |
| Burr height | ≤ 0.05 mm | ≤ 0.02 mm deburred |
| Camber | ≤ 1.0 mm/m | ≤ 0.5 mm/m |
| Edge condition | mill slit | round / deburred / drawn edge |
| Thickness tolerance | EN 485-3 normal | special class ±1 % |
| Coil set / twist | controlled by tension levelling | stress-relieved anneal |
Buyer pain point solved: feeding problems on progressive dies and winding machines almost always trace back to camber and burr, not alloy. Specify the premium column and we laser-measure every delivered coil — with the measurement report attached to the certificate.
Strip Weight, Coil Build-Up & Container Loading
Freight and inventory planning numbers buyers ask for before the PO:
| Strip size (mm) | Weight per 100 m (kg) | Typical slit coil (kg) | Coils per 20 ft container |
|---|---|---|---|
| 0.3 × 25 | 20.3 | 100–200 | ~150 coils |
| 0.5 × 50 | 67.8 | 200–400 | ~80 |
| 0.8 × 100 | 217 | 300–600 | ~50 |
| 1.0 × 125 | 339 | 400–800 | ~38 |
| 1.5 × 200 | 813 | 600–1,200 | ~24 |
| 2.0 × 300 | 1,626 | 1,000–2,000 | ~14 |
| 3.0 × 400 | 3,252 | 1,500–3,000 | ~8 |
Weight formula: kg/m = thickness (mm) × width (mm) × 0.00271. The full formula set for every product form is in our aluminum weight calculation guide.
From Master Coil to Your Slit Width — One Traceable Heat
HXM strips are slit from coils rolled in our own mill — not traded semis from a third party. The advantage shows up in your certificate file: one heat number links casting chemistry, rolling mechanicals and slit-width measurement from melt to delivery.
Where 5083 Strip Wins — Application by Application
| Application | Typical size | Why 5083 strip |
|---|---|---|
| Cable armouring for marine & offshore | 0.3–0.8 mm × 10–32 mm | withstands splash-zone corrosion; interlocks without cracking (O temper) |
| Marine panel stiffeners & edge trims | 1.0–3.0 mm | same alloy as the 5083 plating it joins — no galvanic mismatch |
| Transformer & reactor case components | 0.5–2.0 mm | non-magnetic, corrosion-proof housings for humid environments |
| Stamped brackets & clips (marine/industrial) | 0.4–3.0 mm, H32/H34 | strength holds threads and fasteners better than 5052 |
| Gaskets & shims | 0.15–0.5 mm | stable at temperature, won’t corrode against steel flanges |
| Springs & retaining parts | 0.3–1.5 mm, H18 | high work-hardened strength |
| Honeycomb edge closeouts | 0.3–1.0 mm | pairs with our honeycomb panel production |
Forming, Stamping & Welding 5083 Strip
Process guidance that saves buyers weeks of trial and error:
| Process | Guideline for 5083 strip | Watch out for |
|---|---|---|
| 90° bend, O temper | radius ≥ 1.5 × thickness | keep bend axis transverse to rolling direction |
| 90° bend, H32 | radius ≥ 2.5 × thickness | heat-soften for tighter radii |
| Deep drawing | O temper only, slow speeds | blank holder pressure — 5083 galls more than 5052; use proper lubricant |
| Stamping, H32/H34 | clearance 8–10 % of thickness | work-hardening raises punch wear vs 5052 |
| MIG/TIG welding | ER5356 or ER5183 filler | thin strip distorts — fixture and skip-weld |
| Anodising | anodises cleanly; slightly greyer than 6061 | matte match against other alloys is imperfect |
Deeper process guides: bending & forming best practices · welding fundamentals in our welding guide · gauge-to-thickness conversion for cross-referencing customer drawings.
Quality Control — Certificates You Can Audit
| Checkpoint | Method | Frequency |
|---|---|---|
| Chemistry | OES spectrometry | every heat |
| Mechanicals | tensile test per temper/gauge | every batch |
| Width & thickness | laser measurement | 100 % online + report |
| Burr height | optical profilometry | start/end of every slit coil |
| Surface | visual + eddy current | 100 % |
| Traceability | heat no. on coil tag + certificate | 100 % |
The measurement report ships with the EN 10204 3.1 certificate — so incoming inspection at your plant takes minutes, not days.
Coil Packing & Export Logistics
- Moisture-barrier wrap + desiccant; coils sealed to survive 40+ days at sea.
- Vertical “eye to sky” or horizontal eye-to-side packing per your unloading setup.
- Wooden pallets/crates ISPM-15, steel-strapped, coil OD protected with edge rings.
- Slit-coil labels: alloy, temper, thickness × width, heat number, net weight, HXM coil ID.
- Container plans provided before loading — 20 ft to 25 t, mixed widths balanced for axle-safe unloading.
- Incoterms FOB / CIF / DAP; documents include MTC, COO, invoice and packing list.
Strip Pricing Drivers & the 8-Point RFQ
| Price factor | Impact | Optimisation |
|---|---|---|
| LME aluminium | +/-10–15 % monthly swing | frame agreements with LME formula |
| Slit width count | each new width = knife setup | group widths; buy from running stock |
| Thickness class | thinner gauges cost more per kg | standard steps 0.3/0.5/0.8/1.0/1.5/2.0/3.0 mm |
| Premium edge/deburr | +3–6 % | only where feeding demands it |
| Tolerance class | +2–5 % for ±0.02 mm | reserve for die-critical widths |
| Order size | LCL carries premium | 500 kg MOQ; container = best rate |
For a firm quote in 24 hours, send:
- Alloy 5083 + temper (or application — we’ll specify)
- Thickness × width (and tolerance class needed)
- Coil weight / ID / OD preferences
- Application + environment (indoor, marine, splash zone)
- Certificate needs — 3.1 MTC minimum; laser report, class certs?
- Edge condition — slit / deburred
- Destination port + Incoterm
- Required delivery date
Why Buy 5083 Strip from HXM
- Slit from our own master coils — one heat trace from melt to your 12 mm slit width, no re-seller certificate mismatches.
- Laser-verified tolerances — ±0.05 mm standard, per-coil measurement report included.
- Mixed-alloy containers: 5083 strip alongside 5052 strip, 5083 coil, 5083 sheet/plate and tube in one shipment.
- Marine pedigree: same H116/H321 production system behind our class-certified plate.
- 24-hour quotes with honest tolerance pricing — no surprise adders after the PO.
Frequently Asked Questions About 5083 Aluminum Strip
What width tolerance can HXM hold on 5083 strip?
±0.05 mm is standard on all slit widths; ±0.02 mm is available for die-critical applications. Every coil is laser-measured and the report ships with the mill certificate.
What is the thinnest 5083 strip you produce?
0.15 mm is our standard minimum for 5083. Below that, consider 8011/8021 foil or a 5052 strip at heavier gauge — 5083’s work-hardening makes ultra-thin gauges technically possible but rarely economic.
5083 strip vs 5052 strip — which should I buy?
Choose 5083 when the part is load-bearing or sits in a splash/immersion zone: it delivers roughly 30 % more strength at equal temper. Choose 5052 for general forming where the extra strength isn’t needed — it’s more formable and costs less. Comparison guide: 5052 vs 5083 for marine applications.
Which temper works for deep drawing 5083 strip?
O temper only. 5083 work-hardens quickly, so H32 and above will crack on deep draws. For severe drawing applications, 5052-O or 3003-O draw more forgivingly — send the part drawing and our engineers will confirm.
Can 5083 strip be welded without losing corrosion resistance?
Yes. Weld with ER5356 or ER5183 filler; the joint retains the alloy’s inherent seawater corrosion resistance. The heat-affected zone softens to near-O strength — design weld joints accordingly.
Do you supply deburred or rounded-edge strip?
Yes — deburred edge (burr ≤ 0.02 mm) and rounded/drawn edges are available on request for winding, armouring and edge-contact applications. Add roughly 3–6 % to strip price.
What is the MOQ for a custom slit width?
500 kg per width-thickness combination. If your width can be slit from one of our running stock master coils, trial quantities can be smaller — ask our sales desk for current running widths.
How are slit coils packed for export?
Moisture-barrier wrapped with desiccant, on ISPM-15 wooden pallets or in crates, steel-strapped with edge protection, and labelled with alloy/temper/size/heat number. Container loading plans are sent before shipment.
What certificates come with 5083 strip?
EN 10204 3.1 mill certificate with actual chemistry and mechanicals, plus the slit-width laser measurement report. Marine class certificates (DNV/ABS/LR/BV/CCS) are available for offshore armouring orders.
Can you match 5083 strip to the plate or coil already in my build?
Yes — strip is slit from the same 5083 production system as our plate and coil, so heat-to-heat chemistry and temper logic stay consistent across your assembly. One certificate system covers all forms.
What is the lead time for custom 5083 strip?
12–25 days production depending on width and temper, plus sea transit 25–35 days. Widths slit from running stock masters can ship significantly faster — check availability before planning your production run.
Is 5083 strip suitable for transformer winding cores?
For case components, brackets and busbar supports, yes — it’s non-magnetic and corrosion-proof. For the winding conductor itself, electrical-grade alloys (1350, 1050, 1060) or 3003 transformer strip are the correct choice; 5083’s high Mg hurts conductivity.
How much does 5083 strip weigh per metre?
Weight (kg/m) = thickness (mm) × width (mm) × 0.00271. A 1.0 × 100 mm strip runs 0.271 kg/m. Full formulas in our aluminum weight calculation guide.
Does 5083 strip anodise well?
Yes — it anodises cleanly with good film hardness. Expect a slightly greyer tone than 6061 or 5052; for colour-matched cosmetic parts, sample-anodise first.
Can I get 5083 strip in small trial coils?
From running stock widths, yes. Fully custom widths carry the 500 kg MOQ because each new width requires knife setup on the slitter. Stocked widths change weekly — ask for the current list.
What's the price difference between 5083 and 5052 strip?
Typically 10–20 % higher for 5083 at equal gauge and temper, driven by higher magnesium content and slower rolling. Check our 2026 aluminum price guide for the LME-linked pricing logic behind quotes.
Related Strip Products & Guides
- 5052 Aluminum Strips · 5154 Strips · 5056 Strips · 3003 Strips · 6061 Strips
- 5083 Aluminum Coils — the master-coil source of this strip
- 5083 Sheets & Plates · 5083 Tubes · 5083 Bars
- Aluminum Strip: Complete Guide — alloys, tempers, tolerances & sourcing
- Aluminum Coil: Complete Guide — the upstream form
- 5083 Marine Grade Aluminum Guide · 5052 vs 5083 Buyer’s Guide
- Aluminum Busbar Guide · Bending & Forming Guide · Gauge Thickness Guide
- Aluminum Price Trends 2026 · Weight Calculation Guide · Sourcing Aluminum from China
- Corrosion Resistance Guide · Temper Designations Explained · Mechanical Properties Chart
- All Aluminum Strips · Aluminum Coils · Aluminum Sheets
- All HXM Products · Contact the Factory
Get Your 5083 Strip Quote in 24 Hours
Send the 8-point RFQ above — or just the part drawing and monthly volume. Firm LME-referenced pricing, tolerance capabilities and coil measurement reports within 24 hours.